Zhuohang Precision Machining Factory

Custom Machining Parts

Custom Machining Parts — aluminum, steel, brass and plastics from Dongguan, China. Tolerances: ±0.003 mm milling, ±0.002 mm turning — ISO 9001 / IATF 16949 verified.

Custom machining parts start with the material, and the material is rarely a default.

At a glance
  • Sourcing CNC machining? The test is not the tolerance printed on a brochure — it is whether the shop can hand you a CMM report for the exact feature you are buying, with the band, the sample size and the study window all named.
  • What CNC machining is: a subtractive process — a cutter removes material from a workpiece along a programmed toolpath until the geometry, tolerance and surface finish on the drawing exist.
  • A 6,800 m² floor of named equipment — Mazak, Brother, Tsugami, Star and Citizen machines (3-axis 50+, 4-axis 20+, 5-axis 20+, 25+ lathes, 7+ grinders, 20+ inspection instruments).
  • Tolerance: ±0.003 mm, turning ±0.002 mm, grinding ±0.002 mm — verified on Hexagon CMMs. Capability is reported per characteristic: Ppk ≥ 1.67 in the initial study and Cpk ≥ 1.33 in production on key and special characteristics (≥ 1.33 on general characteristics). Every report names the feature, its tolerance band, the sample size, the sigma method, and the study window.
  • Three certificates — ISO 9001:2015, IATF 16949:2016 (design excluded) and ISO 14001:2015, all held by Dongguan Zhuohang Ltd, the entity that invoices you.
  • Order terms: MOQ 1 piece, lead times of roughly 3 / 7 / 30 days depending on complexity.

What are custom machining parts?

Custom machining parts are parts machined to your drawing from the alloy you specify — no catalog, no tooling, no minimum beyond one piece. The material decision comes first because it sets the machining speed, the finish options and the price. This Dongguan plant cuts aluminum, steel, stainless, brass, copper and titanium, with every lot XRF-checked at the door.

CNC machining is the subtractive manufacturing of parts on computer-numerically-controlled milling, turning, and grinding equipment. A cutter removes material from a workpiece along a programmed toolpath to produce a part that meets a drawing-defined geometry, tolerance, and surface finish. "CNC" means the tool path is numerically controlled rather than hand-operated.

The rest of this guide turns that definition into a buyer's checklist for this shop — what to verify before you commit, and how the numbers on the drawing actually reach the part.

The discipline separates into milling (the cutter rotates and the workpiece is fed; prismatic geometry), turning (the workpiece rotates and the tool is fed; rotational geometry), and precision grinding / wire EDM (the tightest tolerances on critical features). A plant that produces CNC machined parts end-to-end runs all three.

The output of CNC machining is a part that meets the drawing — geometry, tolerance, surface finish, and material certificate — and is documented to a quality plan (FAI for general work, PPAP for automotive-bound parts, IMDS for material data). That is the answer to "what is CNC machining": a numerically-controlled subtractive process that produces a part to a drawing, with the quality documentation that lets the part enter an assembly.

The selection chain, at a glance
  • Function first. Lightweight strength → aluminum; strength and wear → steel; corrosion → stainless; conductivity → brass/copper; strength at low weight → titanium.
  • Material drives process. Aluminum cuts fast; stainless runs slow; copper is soft; titanium is slow and tool-demanding — each material sets its own machining approach.
  • Material drives finish. Aluminum anodizes; steel plates or heat-treats; copper gets silver or gold plating; the material narrows the finishing options.
  • Evidence, not claims. ±0.003 mm (milling) / ±0.002 mm (turning) machining, ±0.002 mm grinding, XRF material verification, and ISO 9001 + IATF 16949 process control back every decision.

How do you choose the right material for a custom machining part?

Choose the material from the part's function, not from what you ordered last time. A bracket that holds a lens needs stiffness at low weight; a shaft that runs against a seal needs strength and wear resistance; a fitting that sits in seawater needs corrosion resistance; a bus bar needs conductivity. These are different requirements, and no single alloy answers all of them.

The decision runs through three questions in order. First, what load does the part carry? If it is structural and weight matters, you are looking at aluminum or titanium. If it carries load and gets pushed hard, steel. Second, what environment does it live in? Moisture, chemicals, or salt pushes you toward stainless steel or a plated finish. Third, what does the part touch? Electrical current points to copper or brass; a mating surface that must not gall points to a specific alloy pair.

Answer those three and the material choice mostly makes itself. The sections below run each family through the same lens so you can compare them side by side before you commit a drawing.

Three second-order effects follow from this ordering, and they are the ones that cost real money when ignored. The first is machinability: a material that is twice as strong is usually harder to cut, so the same geometry costs more in one alloy than in another. The second is finish compatibility: the surface treatment you want only exists on some alloys — you cannot anodize steel, and you rarely chrome-plate aluminum. The third is lead time: a material with an outsourced step, such as titanium stress relief, lands in a longer delivery tier no matter how fast the cutting goes.

The way to check your own decision is to reverse it. Write down the finish you want first, then ask whether the material supports it; write down the lead time you need, then ask whether the material allows it. If either answer is no, the material is wrong no matter how well it machines.

If you are starting cold, run the three questions as a filter. Does the part carry a load that weight matters against? That points to aluminum or titanium. Does it face moisture, chemicals, or salt? That points to stainless or a plated steel. Does it carry current or move heat? That points to copper or brass. Most parts land in one of those three buckets on the first pass, and the sections below give you the detail to confirm the pick.

If the part must be…Start with…Why
Lightweight and stiffAluminum (6061, 7075)Good strength at low weight, machines fast, anodizes well
Strong, wear-resistant, heat-treatableSteel (1045, 4140) or stainlessHigh strength; carburizing and nitriding add a hard surface
Corrosion-resistantStainless steel (303, 316, 316L)Corrosion resistance is in the alloy, not a coating
Electrically or thermally conductiveBrass (C360, H62) or copper (C110)Carries current and heat; brass also machines easily
Strong at the lowest possible weightTitanium (TA2, TC4)Strength per unit weight, corrosion-resistant, but slower to machine

What does aluminum give you, and when is it the wrong pick?

Aluminum is the default for a reason: it is light, it machines quickly, it costs less than most metals, and it takes anodizing beautifully. If your part is a housing, a bracket, a heatsink, or any structural piece where weight matters more than ultimate strength, aluminum is almost always the first material to try.

The grades change the behavior. 6061 is the general-purpose workhorse — machinable, weldable, and predictable. 7075 is stronger and is the choice when an aluminum part has to carry real load, at the cost of being a little less forgiving to finish. Both anodize, both can be held to ±0.003 mm (milling) / ±0.002 mm (turning), and both are on our floor every day.

Aluminum is the wrong pick when the part faces sustained wear, high heat, or corrosive chemicals. Anodizing helps, but it is a thin oxide layer, not a substitute for a material that is inherently corrosion-resistant or heat-tolerant. If the part rubs against a mating component or sits in an aggressive environment, move up the chain to steel or stainless instead of asking aluminum to do a job it was never built for.

The two workhorse grades separate cleanly on public datasheet numbers, and the table below is why you pick one over the other.

Property (typical)6061-T67075-T6
Density2.70 g/cm³2.81 g/cm³
Tensile strength (approx.)310 MPa572 MPa
Yield strength (approx.)276 MPa503 MPa
Corrosion resistanceGoodModerate
AnodizingExcellentGood

Read the table as a trade, not a ranking. 6061 wins on corrosion and anodizing, which is why it is the default for housings that must take a clean colored finish. 7075 wins on strength, which is why it carries load when a part has to stay aluminum but work hard. Both machine well and both anodize — the difference is which requirement you are actually buying.

When does a steel part earn its place over aluminum?

Stainless-steel component turned on a CNC lathe, with the workpiece held in a 3-jaw chuck.

Steel earns its place the moment strength or wear becomes the controlling requirement. A pin, a shaft, a gear, a fastener boss, or any part that carries load repeatedly and must not deform is steel territory. Steel is stronger than aluminum, and — this is the part buyers often overlook — it can be heat-treated to change its surface and its hardness, which aluminum generally cannot.

Carburizing and nitriding are the two heat treatments that matter most for wear parts. Carburizing adds carbon to the surface so it can be hardened while the core stays tough; nitriding does something similar with nitrogen at a lower temperature. Both give you a part that is hard where it rubs and tough where it carries load. If your drawing says "hardened" or "wear-resistant," you are in this territory, and the finish decision becomes a heat-treatment decision rather than a plating decision.

Steel parts almost always need a surface treatment, because bare steel rusts. Zinc, nickel, and chrome plating, powder coating, and painting are the standard answers, and the choice depends on whether you are fighting corrosion, appearance, or both.

Within steel, the grade splits by what you need the part to survive. Low-carbon 1018 is easy to machine and weld, so it suits brackets and light structural work. Medium-carbon 1045 adds strength and responds well to hardening. Alloy steel 4140 is the heat-treatable workhorse for shafts, gears, and tooling — it can be through-hardened or case-hardened to take a hard, wear-resistant surface while keeping a tough core. The grade, not the word "steel," is what decides whether a wear part survives its first hundred thousand cycles.

When does stainless steel justify its higher cost and longer lead time?

Stainless steel costs more and machines slower than aluminum or mild steel, so it has to earn its place. It earns it when the part lives in moisture, washdown, or chemical exposure, or when hygiene and cleanability matter. Food-contact fittings, medical instrument parts, and marine hardware are the classic cases.

The important distinction for you is where the corrosion resistance comes from. In stainless, it is in the alloy itself — the chromium forms a self-healing oxide layer — not in a coating that can chip or wear off. That is why 316 and 316L are the go-to grades for aggressive environments: their protection is intrinsic, not applied. If your part has a plating that can scratch through to bare metal, that scratch becomes a corrosion site; a stainless part does not have that failure mode.

The trade-off is real and worth planning around. Stainless is harder to machine than aluminum, so it runs slower and can cost more per part. 303 is the free-machining grade when you need stainless properties but easier cutting; 316L is the choice when corrosion resistance is the whole point. Surface finishing is usually a mechanical polish or passivation-free brushed finish rather than a plating.

The grade inside "stainless" changes both machining and corrosion. 303 is free-machining — it cuts cleanly and holds tolerance, which means it shows up in threaded fittings and small turned parts. 304 is the general-purpose workhorse. 316 and 316L add molybdenum, which is what resists chlorides and salt, so they are the call for marine and washdown duty. The "L" in 316L means low carbon, which improves weldability and resists a corrosion mode called sensitization along the weld. When a drawing just says "stainless," that is the first thing to tighten up.

When do brass and copper make sense for machined parts?

Brass and copper earn their place on one word: conductivity. If the part carries electrical current or moves heat, you are in their territory. Bus bars, contacts, terminals, heat spreaders, and RF components are where copper and brass show up, and no amount of aluminum or steel will do that job as well.

The two metals behave differently on the machine. Brass — free-machining grades like C360 and H62 — cuts beautifully, holds tight tolerances easily, and leaves a clean finish, which is how it is a favorite for small precision fittings and threaded inserts. Copper is softer and gummier, which makes it trickier to hold to tight tolerance, but its electrical and thermal conductivity is what you are paying for, and it is the standard for current-carrying parts.

Both tarnish in air, so the surface finish is usually a plating — silver for conductivity and appearance, gold for the best contact resistance, or nickel for a protective barrier. The finish here is not decoration; it directly affects how the part performs electrically.

The conductivity numbers make the case on their own. Copper conducts electricity at roughly 5.96 × 10⁷ S/m, while aluminum manages about 3.5 × 10⁷ S/m and steel is far lower. Brass sits below copper on conductivity but machines far more easily, which is the trade that makes C360 the default for small threaded conductive fittings where the part is more connector than conductor. When pure conductivity is the whole point, C110 copper wins; when you need a part that threads cleanly and still carries signal, brass earns its keep.

When is titanium worth the difficulty and the lead time?

Titanium is the material you choose when the part must be strong, light, and corrosion-resistant all at once, and when you are willing to pay for all three. Aerospace brackets, medical implants, high-end racing components, and anything where every gram counts against a load requirement is titanium territory.

Be honest about the trade-offs before you commit, because titanium is genuinely harder to machine. It is strong for its weight and resists corrosion, but it cuts slowly, it is demanding on tooling, and stress relief for some grades has to go to a qualified outside partner because it requires temperatures above what an in-house oven reaches. In practice, a titanium part will usually land in the longer lead-time tier, and it will cost more than the steel or aluminum part that does the same job.

The decision rule is simple: if you do not actually need the strength-to-weight ratio, do not pay for titanium. If you do need it, specify the grade carefully — TA2 for general corrosion work, TC4 (Grade 5) for strength — and plan the lead time from the start rather than discovering it at the end.

The density numbers are why this material gets used at all. Titanium runs about 4.43 g/cm³ against steel's roughly 7.85 g/cm³, so a titanium part can be nearly half the weight of the same steel part while holding comparable strength — the entire reason it appears in aerospace and racing. Against aluminum's 2.70 g/cm³ it is heavier, but it beats aluminum on strength and on corrosion in aggressive environments. That middle position, lighter than steel and stronger than aluminum, is what you are paying for, and it is a narrow band that only some parts actually need.

How does the material drive the machining process?

Once the material is chosen, the process mostly follows. You do not machine stainless the way you machine aluminum, and the shop you pick should be able to explain the difference, because the difference is where scrap and lead-time surprises come from.

Aluminum machines fast and forgiving, which makes it cheap to prototype and to hold tight tolerances on. Stainless runs slower and can work-harden, so feeds and speeds tighten up and the per-part cost rises. Copper is soft and gummy, which demands careful tooling to hold dimensions. Titanium is slow and hard on cutters, which explains why it lands in the longer lead-time tier. Steel sits in the middle on machining, but its real process story is heat treatment after the cut, not the cut itself.

This is also where our floor matters. With 100+ production machines spanning 3-axis, 4-axis, and 5-axis milling, turning, mill-turn, and grinding, the right process for the material is already in-house rather than something that gets subcontracted out and adds days. A material-appropriate process, run under one roof, is the difference between a quoted lead time and a real one.

The second-order effect most buyers miss is that machinability does not scale with strength — it runs almost backward. Aluminum is weak and machines fast; titanium is strong and cuts slow; copper is soft yet gummier than steel to hold on tolerance. That is why a material decision made in a vacuum, without a process conversation, produces surprises on the invoice. The shop that can tell you why your alloy cuts the way it does is the shop that has already run it, and running it is what turns a quoted lead time into a kept one.

How does the material drive surface finishing?

Precision CNC turning center workshop for turned custom machining parts
Turning centers for round parts across all material families
Mazak VCE-570CL three-axis machining centres on our production floor in Hengli, Dongguan.
3/4/5-axis milling centers machining multiple materials

The finish is the last decision in the chain, and it is fully constrained by the two decisions before it. You cannot anodize steel, and you rarely plate aluminum with zinc. Each material family comes with its own finishing menu, and picking the right finish is a matter of matching it to the material and the part's environment.

MaterialTypical finishesWhat the finish is for
AluminumStandard anodizing, hard anodizing, brushing, mirror polishCorrosion resistance, wear resistance, color, appearance
SteelZinc / nickel / chrome plating, powder coat, paint, carburizing, nitridingRust protection, wear resistance, appearance
Stainless steelBrushing, mirror polishCleanability, appearance; corrosion is already in the alloy
Brass / copperSilver / gold / nickel platingConductivity, contact resistance, tarnish protection
TitaniumAnodizing, polishingColor, appearance; the alloy already resists corrosion

Plan the finish into the lead time. A finish is a process step, not an afterthought. Anodizing, plating, and heat treatment all add days on top of machining, so a part with finishing usually lands in the longer lead-time tier. If you know the finish up front, it gets scheduled in parallel instead of bolted on at the end.

Surface roughness is the other half of the finish callout, written as Ra in micrometres. A raw machined surface is often around Ra 3.2 µm; a general machined finish lands near Ra 1.6 µm; a fine or ground finish is Ra 0.8 µm; and a polished finish can go to Ra 0.4 µm and below. Writing the Ra on the drawing matters because it changes the process — you do not get Ra 0.8 from a milling cutter alone, you get it from grinding or polishing, and each step adds time and cost. When a drawing leaves Ra blank, the shop guesses, and a guessed finish is a guessed price.

What belongs in a complete material-and-finish spec?

Custom machined parts in aluminum and steel
Finished parts in aluminum, steel, and stainless

The single most common reason a custom machining part comes back wrong is a spec that names a metal but not a grade, and a finish that says "nice surface" instead of naming a process. Both are free to fix, and both are the difference between a part that fits and a part that gets re-quoted.

  • Name the grade, not just the metal. "Aluminum" is not a material; 6061-T6 is. Write the full callout so there is nothing to assume.
  • Name the finish as a process. "Anodize clear, Type II" or "zinc plate, then black", not "make it shiny."
  • Flag the critical dimensions. Tolerance the two or three features that control function, and leave the rest at a general default.
  • State the environment. One sentence about where the part lives — indoor, outdoor, salt, washdown — lets the shop confirm the material and finish will survive it.
  • Ask how the material is verified. A shop that XRF-checks incoming stock against the mill certificate is protecting you from mixed lots at the door.

Send that package to [email protected] and you get back a quote plus a material and finish recommendation, and, if your choice has a cheaper or more durable alternative, a note telling you so before you commit.

What tolerance classes and surface finish callouts should your drawing use?

A drawing that leaves tolerance and finish blank forces the shop to guess, and a shop that guesses prices the guess conservatively. The standard way to remove the guess is to write a general tolerance class from ISO 2768, then tighten only the few dimensions that control function.

ISO 2768 gives four classes — fine (f), medium (m), coarse (c), and very coarse (v) — that apply to every dimension not individually toleranced. The class you write tells the shop how much any unlabeled dimension may wander. To take a common band, for a nominal dimension in the 30–120 mm range, class m allows ±0.3 mm, class f allows ±0.15 mm, and class c allows ±0.8 mm. Tighter classes cost more because the process has to work harder to hold them, which is exactly why you should tighten only what matters.

CalloutWhat it meansWhen to use it
ISO 2768-mGeneral tolerances for unlabeled dimensions, medium classDefault for most machined parts
ISO 2768-fFine general tolerancesParts with many closely related features
Ra 3.2 µmStandard machined surfaceNon-sealing, non-wear surfaces
Ra 1.6 µmGeneral machined finishMating surfaces, o-ring grooves
Ra 0.8 µmFine or ground finishBearing seats, sealing faces

The rule that ties this back to the selection chain: the material and the finish set a floor on the roughness you can reach, and the tolerance class sets the cost of holding the size. Pick the class for the function, not for the drawing's dignity — over-tolerancing a non-critical dimension is how a cheap part becomes an expensive one for no reason.

What DFM rules keep a machined part affordable?

Most part cost is decided at the drawing stage, before anyone quotes. A feature that looks innocent in CAD can double the machining time, and the rules that prevent that are design-for-manufacturability (DFM) rules. They are general practice, not factory-specific claims, and they apply to any shop you send the drawing to.

FeatureRule of thumbWhy it matters
Wall thicknessKeep walls above roughly 0.8 mm in aluminum, more in soft plasticsThin walls flex, chatter, and distort during cutting
Hole depthKeep drilled holes to about 4× diameter before special toolingDeeper holes wander and break drills
Internal cornersSpecify as large a radius as the design allowsA cutter leaves a radius; sharp internal corners need slow EDM work
Thread depthAbout 1.5× diameter holds a thread's full strengthDeeper threads add time without adding much strength
UndercutsAvoid unless the function requires themUndercuts need special tooling and extra setups

The payoff of these rules lands inside the selection chain too. A material that is hard to machine magnifies every DFM violation — a deep hole that is merely annoying in aluminum becomes a scrap risk in stainless or titanium. When the material, the process, and the geometry are designed together, the part is cheaper and arrives on time; when they are designed separately, the invoice tells the story.

How do the main material families compare side by side?

By now the pattern should be clear: no single alloy wins every requirement, and the right pick is the one that matches the load, the environment, and what the part touches. The table below puts the families next to each other on the properties a buyer actually weighs.

MaterialDensity (g/cm³)StrengthMachinabilityCorrosionTypical finish
Aluminum 60612.70ModerateFastGoodAnodizing
Aluminum 70752.81HighFastModerateAnodizing
Carbon / alloy steel~7.85HighModeratePoor (needs plating)Plating, powder coat
Stainless 303 / 304 / 316~7.9HighSlowExcellentPolish, passivation
Brass / copper8.4–8.9Low–moderateBrass fast, copper gummyGoodSilver / gold / nickel
Titanium4.43Very high for weightSlow, tool-demandingExcellentAnodizing, polishing

Read the table by column, not by row. If weight drives the decision, follow the density column. If schedule drives it, follow the machinability column. If the part lives outdoors, follow the corrosion column. The material that wins two of the three columns you care about is usually the right one, and the finish column is the reminder that every material already points at its own surface treatment.

What does heat treatment change, and when does steel need it?

Heat treatment is the step that lets a steel part be hard where it wears and tough where it carries load — a combination no single unhardened alloy can give you. It is also the step most buyers forget to schedule, which means a "hardened" callout so often arrives late.

TreatmentWhat it doesWhen to specify it
Through-hardeningHardens the whole cross-sectionParts that wear uniformly and carry moderate load
CarburizingAdds carbon to the surface, then hardens it while the core stays toughGears, pins, shafts that need a hard skin and a ductile core
NitridingAdds nitrogen to the surface at lower temperature, less distortionParts that must stay dimensionally stable and resist wear
Stress-relief agingRemoves internal stress after rough cutting or weldingParts that would otherwise warp during finishing

Heat treatment matters to the selection chain because it changes the finish decision. A carburized or nitrided surface is its own finish — hard and wear-resistant — so the part may not need plating at all. But hardening also moves the final sizing to grinding, since hardened steel is too hard to cut cleanly. That is the real cost of the "hardened" callout: not the oven, but the grind that has to follow it.

What is the difference between standard and hard anodizing?

Anodizing is the default finish for aluminum, but "anodize" on a drawing hides two different processes with two different jobs. Standard anodizing (often called Type II) builds a thin oxide layer for corrosion resistance and color; hard anodizing (Type III) builds a much thicker, denser layer for wear resistance.

PropertyStandard anodizing (Type II)Hard anodizing (Type III)
Typical thicknessThin, measured in a few micrometresMuch thicker, commonly tens of micrometres
Primary jobCorrosion resistance and colorWear and abrasion resistance
Dimensional effectMinimalThicker layer must be allowed for in tolerance
Typical useHousings, brackets, cosmetic partsSliding surfaces, pistons, wear plates

The distinction matters because hard anodizing grows the part's surface by a measurable amount, and that growth has to be designed into the tolerance stack. A bearing bore that must stay round after hard anodizing is a different drawing than a cosmetic cover that just needs to look clean. Name which type you mean and the shop can hold the dimension; leave it blank and you get a guess.

How does the selection chain play out across real industries?

The same function-material-process-finish sequence produces different answers in different industries, which is how a good material conversation starts with what the part actually does, not with what industry it belongs to.

E-bike drivetrains push strength at low weight, so aluminum and titanium show up in brackets and sprockets, with hard anodizing for wear. Medical instrument parts push corrosion and cleanability, so 316L and 304 dominate, with a brushed or mirror finish for cleanability rather than plating. Robotics and automation split the difference: aluminum for structural links, steel for joints and shafts that carry repeated load, and hard anodizing or plating on the wear surfaces. Semiconductor and electronics tooling leans on copper and brass for thermal and electrical paths, with gold or silver plating where contact resistance decides performance.

The pattern across all four is the same: the environment picks the material, the material picks the process, and the finish closes the loop. No industry is special enough to skip the chain — they just weight its links differently.

When does the material-process-finish chain fail, and what signals it early?

The selection chain fails in predictable ways, and most of them are visible in the RFQ before a single part ships. The most common is the unspecified-grade callout — a drawing that says "aluminum" or "steel" and leaves the alloy to whoever quotes it. That is not a material decision; it is a coin flip.

Watch for four signals that the chain was skipped. A quote that ignores the environment — you say "marine" and nothing about corrosion comes back — means the material was picked by habit, not function. A finish listed as decoration, like "make it shiny," will be re-quoted once the part rusts or fails contact resistance. A lead time that ignores the material means the shop is guessing, because titanium and stainless genuinely take longer than aluminum. And no verification story means the alloy callout is a hope, not a fact.

The reverse view is the fastest audit: assume every vague field on your drawing will be filled in with the cheapest available option, then ask whether that option still works in service. If it would not, the spec is not done.

What should you ask a supplier before you commit?

Before you send a drawing, run the same five questions against any shop — including this one — and hold the answers in writing. They separate a manufacturer that runs the selection chain from a desk that only forwards your file.

Notice that none of these questions asks for a price first. Price is the dependent variable: it follows from the material, the process, the finish, and the evidence behind them. Get the chain right and the price is honest; skip the chain and no discount makes the part work.

For the step-by-step routine that runs the same check before you send a drawing — entity first, then material range, process mix, and verification evidence, in thirty minutes — see the online supplier screening guide.

How do material, process, and finish set the lead time?

Lead time is not a single number the shop invents; it is the sum of the chain's steps. A simple aluminum part that needs no finishing can ship in about 3 days. Add a surface finish or a heat-treatment step and the same geometry moves into a longer tier — roughly 7 or 30 days depending on how many steps stack up. The reason is that finishing and heat treatment are processes with their own dwell time, and they run after the cutting stops.

This is why the material decision and the finish decision belong in the RFQ, not in a follow-up. If you lock the finish up front, you let the shop schedule it in parallel with machining. If you add "oh, and anodize it" after the quote has already committed to a date, you are the one who watches the date slip. The tiers — roughly 3, 7, or 30 days — are honest because they follow the chain, not the other way around.

What drives the cost of a machined part?

Cost follows the same chain as everything else on this page, and knowing the drivers is how you keep a quote from surprising you. The table below is the short list, in rough order of leverage.

Cost driverHow it actsWhat you control
MaterialAlloy price and how hard it is to cutPick the alloy the function needs, not the one on hand
ToleranceTighter tolerances add setup and inspection timeTighten only the dimensions that control function
GeometryDeep pockets, thin walls, and small radii add timeApply DFM rules before you send the drawing
FinishPlating and anodizing add process stepsName the finish as a process, and plan it in
QuantitySetup cost spreads across more partsQuote in tiers to see where the unit price breaks

There are no fixed prices on this page, and that is deliberate — a part's cost is set by the drawing, not by a rate card. What you control is the spec: a clean material callout, a sensible tolerance class, DFM-friendly geometry, and a finish named as a process. Those four decisions do more to the final number than any negotiation over the hourly rate.

What should a first article inspection verify?

Before a production run, the first article is the proof that the chain held, that the material, the process, and the finish all delivered what the drawing asked. A first article inspection (FAI) measures one part, complete, against the full drawing, and it should check three things in order.

First, the material — the mill certificate and the XRF result, so the alloy is confirmed rather than assumed. Second, the geometry — every dimension and tolerance measured on a CMM, not sampled with calipers. Third, the finish — roughness, coating thickness, and hardness where they apply. When all three pass, the process is released and the rest of the batch is machined to the same settings.

For you, the FAI is the moment to catch a wrong assumption before it becomes a wrong shipment. A part that measures correctly at the first article and looks right in the application is the green light that the selection chain has done its job. Skip the first article and you are betting the whole batch on a chain nobody verified.

Guides

What this shop actually runs

A buyer asking for capability evidence should get a specific answer. The facility behind this guide operates 100+ CNC machines across a 6,800 m2 plant in Dongguan, China, with 100+ staff. The machine list by category:

  • 5-axis machining centres (10+) - Mazak VARIAXIS I-600 (510/910/510 mm travel, 12,000 rpm, 22 kW, 71.6 N·m, 30-tool BT40) and Mazak INTEGREX I-250H S (B-axis 0.0001°, 24 kW, 124 N·m, 38-tool HSK-A63). Built for compound-angle parts, single-setup multi-face prismatic work, and aerospace fittings where datum transfer loss is unacceptable.
  • 3-axis / 4-axis machining centres (50+) - Brother SPEEDIO S500Z2N / S700Z2N (10,000 rpm, 14/21-tool ATC, 0.7 s tool-to-tool, Z-axis 2.2 G) and Mazak VCE-430A L / VCE-570C L (10,000 rpm, 118 N·m, 24-tool ATC). Built for prismatic parts, plates, brackets, housings.
  • Swiss-type turning centres (10+) - Citizen Cincom A20-3F7 (Φ20 mm, 10,000 rpm), TSUGAMI B0206-III / B0205-III (Φ20 mm, 0.1 µm), STAR SR-32JII / SR-32J Type N (Φ32 mm, 8,000 rpm). Built for long, slender rotational parts at ±0.002 mm.
  • CNC turning centres (20+) - HEADMAN T70M/1250 (720 mm swing, 117 mm bore, 3,000 rpm, BMT75 12-station turret). Built for shafts, bushings, flanges up to ±0.002 mm.
  • Wire EDM (5+) - Sodick AQ535L (550/350/300 mm travel, ±20° taper, 800 kg workpiece). Built for hardened tool steel, internal splines, sharp internal corners that milling cannot reach.
  • Inspection: Hexagon CMM + 20+ gauges - Hexagon CMM for coordinate measurement, plus vision system, profilometer, hardness tester, coating thickness gauge, XRF for material verification. The 10:1 rule (gauge 10x more accurate than the band) is applied to every feature.
  • Machine highlights - VARIAXIS I-600: one-setup multi-face 5-axis + MAZA-CHECK auto-calibration; INTEGREX I-250H S: DONE-IN-ONE mill-turn, B-axis 0.0001° + Ai thermal shield; SPEEDIO S500Z2N / S700Z2N: Z-axis 2.2 G + 0.7 s ATC; Swiss-type: guide-bush switchable + 0.1 µm resolution.

Tolerance bands held: ±0.003 mm on CNC milling, ±0.002 mm on CNC turning, ±0.002 mm on precision grinding and wire EDM. Capability indices: Ppk >= 1.67 initial on key characteristics; Cpk >= 1.33 ongoing in production.

Certifications: ISO 9001:2015 (116024/A/0001/UK/En), IATF 16949:2016 (131941/A/0001/SM/En, design clause 8.3 excluded - disclosed openly), ISO 14001:2015 (116024/B/0001/UK/En). Certificates are issued to Dongguan Zhuohang Ltd (USCC 91441900MA4UWT6X39, established 2005).

Service area: Austria, Belgium, the Czech Republic, Denmark, France, Germany, Greece, Hungary, Ireland, Italy, the Netherlands, Spain, Sweden and the United Kingdom in Europe; Brazil, Canada, Mexico and the United States in the Americas; China, Israel, Japan, Singapore and Sri Lanka in Asia; Australia and New Zealand in Oceania; and South Africa in Africa. Based in China, serving customers worldwide.

Contact: Felipe Iglesias, [email protected], +86 13126536955.

Ready to lock in the material and finish for your part?

Send your drawing to [email protected] or call +86 13126536955 for a material, process, and finish recommendation plus a quote.

Frequently Asked Questions

How do I choose the right material for a custom machining part?

In short, Start from the part's function, not from habit. Pick aluminum for lightweight strength, steel for strength and wear, stainless steel for corrosion resistance, brass or copper for conductivity, and titanium when you need strength at low weight.

Which material should I choose for a corrosion-resistant part?

Stainless steel is the usual answer for parts exposed to moisture or chemicals. Grades 316 and 316L resist corrosion well, and their protection comes from the alloy itself rather than a coating, so it does not wear off the way a plated finish can.

Can you anodize aluminum parts?

Yes. We offer standard and hard anodizing for aluminum parts. Anodizing builds a protective oxide layer that resists corrosion and wear and accepts color, which explains why it is the default finish for aluminum housings and structural parts.

How do you verify the material is what I ordered?

Incoming raw stock is checked with a handheld XRF spectrometer against the mill certificate before it reaches a machine. This catches mixed or mislabeled lots at the door, so the alloy you specify is the alloy that gets cut.

Can you machine titanium, and what should I expect?

Yes, we machine titanium in grades such as TA2 and TC4. Titanium is strong for its weight and corrosion-resistant, but it cuts slowly and stress relief above 500 °C is outsourced to a qualified partner, which adds lead time to the longer tier.

What surface finishes do you provide for steel parts?

Steel parts can be zinc, nickel, silver, gold, or chrome plated, powder coated, painted, brushed, or mirror polished. Heat treatment such as carburizing and nitriding is also available for parts that need a hard, wear-resistant surface.

What is your minimum order quantity?

Our MOQ is 1 piece. You can order a single prototype to validate a material and finish choice, then move to production once the first article measures correctly and looks right in the application.

What are your typical lead times?

Roughly 3, 7, or 30 days depending on part complexity and process steps. A simple part ships in about 3 days; a part with surface finishing or heat treatment falls into the longer 30-day tier because the finishing steps add time.

How do I get a material and finish recommendation for my part?

Send your STEP, IGES, or 2D drawing to [email protected] and describe what the part does and the environment it lives in. We reply with a material and finish recommendation plus a quote, usually within one business day.

What do ISO 2768 and Ra mean on a drawing?

In short, ISO 2768 is a general-tolerance standard: write a class (f, m, c, or v) next to it and it applies a tolerance to every unlabeled dimension. Ra is surface roughness in micrometres — Ra 3.2 µm is a standard machined surface, Ra 1.6 µm is a general finish, and Ra 0.8 µm is a fine or ground finish.

How thick should the walls of a machined part be?

In short, Keep walls above roughly 0.8 mm in aluminum and thicker in softer plastics. Thin walls flex and chatter during cutting, which distorts the part and risks scrap.

Which industries do you serve with material and finish selection?

In short, The same selection chain runs across e-bike drivetrains, medical instruments, robotics and automation, and semiconductor or electronics tooling. Each industry weights the links differently — strength-to-weight here, corrosion and cleanability there — but the sequence of function, material, process, and finish is the same.

What is the difference between 6061 and 7075 aluminum?

In short, 6061-T6 is the general-purpose grade: it machines well, welds, and anodizes beautifully. 7075-T6 is stronger but less corrosion-resistant and a little less forgiving to finish.

Can you machine plastic parts as well as metal?

In short, Yes. We machine engineering plastics including ABS, POM, nylon, PTFE, and PEEK for non-metal prototypes, insulators, and low-friction parts.

What does MOQ 1 piece mean in practice?

In short, Our minimum order quantity is 1 piece, so you can order a single prototype to validate a material and finish choice before committing to a production run. That suits teams moving from a first sample into volume, because the first part confirms the selection chain before the batch is locked in.

Why do you ask about the environment when I send a drawing?

In short, One sentence about where the part lives — indoor, outdoor, salt, washdown, or chemicals — lets us confirm the material and finish will survive it. The environment is the question that decides between anodized aluminum, plated steel, and stainless, so it is the fastest way to catch a mismatched alloy before cutting starts.

Do you use MIL-STD-105E or ANSI/ASQ Z1.4 sampling inspection?

In short, MIL-STD-105E is the U.S. military sampling inspection standard published in 1989; it specifies acceptable quality limit (AQL) sampling plans for lot-by-lot inspection.

Standards referenced on this page

  • ASTM B211/B211M-19 — Standard Specification for Aluminum-Alloy Rolled or Cold Finished Bar, Rod, and Wire
  • ASTM A276/A276M-17 — Standard Specification for Stainless Steel Bars and Shapes
  • ISO 9001 — Quality management systems — Requirements

Why choose Zhuohang for Custom Machining Parts?

Because the hard part is not finding a supplier — it is trusting one. Ten checks follow, from a single-part order to what happens if a part is wrong.

  1. Audit the floor. The address is real: a 6,800 m² plant in Hengli, Dongguan, operating since 2005 as Dongguan Zhuohang Ltd (USCC 91441900MA4UWT6X39). We comply with all applicable laws, pay suppliers and wages on time, and support the local community through charitable donations. Our record is publicly verifiable and buyer-side due diligence is welcome.
  2. Three certs, one system. ISO 9001:2015, IATF 16949:2016 (design excluded) and ISO 14001:2015 cover the same floor — prototype or automotive Custom Machining Parts batch, one quality standard.
  3. Tolerances we hold. ±0.003 mm milling, ±0.002 mm turning, ±0.002 mm grinding and wire EDM — each one measured, not claimed.
  4. Machines you can name-check. Mazak VARIAXIS I-600, Mazak INTEGREX I-250H S, and Tsugami, Star and Citizen Swiss lathes — the gear behind tight features.
  5. Numbers, not opinions. Hexagon CMM and vision checks on every lot, with capability reported as Ppk ≥ 1.67 initially and Cpk ≥ 1.33 in production, each with index, stage and sigma method.
  6. When a part is returned as defective. Repair or remake is free of charge, and we cover return shipping both ways.
  7. Shipments that clear. Material certification goes with every order, and the US Section 301 / Section 232 and EU CBAM status is kept current for our HS codes.
  8. Everything under one roof. Milling, turning, mill-turn, grinding and wire EDM share one floor and one quality system, so your Custom Machining Parts parts never stall between vendors.
  9. One part is welcome. Prototype and production share the same program and datum, so the sample you approve is exactly what ships when the order scales.
  10. Quote plus DFM in ~48 hours. The cost-lowering changes to your Custom Machining Parts part are raised before machining begins, so there are no surprises at billing.

Care to put any of the ten to the test? Upload a drawing for a 48-hour quote, or speak to the team in English, Japanese, Portuguese, Spanish, French, Chinese or Cantonese.

Parts, inspection and paperwork